@article{1546c3050ca54e44ac08554c0141b0ef,
title = "Combination of Nanoindentation and Microscopy for the Examination of Aluminum Alloys in Coarse- and Ultrafine-Grained Condition",
author = "Johann Kappacher and Alexander Leitner and Helmut Clemens and Verena Maier-Kiener",
year = "2019",
month = jan,
day = "9",
doi = "10.3139/147.110571",
language = "English",
volume = "56.2019",
pages = "432--442",
journal = "Practical metallography = Praktische Metallographie",
issn = "0032-678X",
publisher = "Walter de Gruyter GmbH",
number = "7",
}