Abstract

Quasi-static delamination resistance tests under Mode I, Mode II and Mixed-Mode I/II loading are performed on unidirectional (UD) glass fiber (GF) and carbon fiber (CF) reinforced polymer laminates manufactured with the same epoxy matrix. Compared to the CF-, the GF-epoxy laminate has a higher fracture toughness under all loading modes. Fracture toughnesses differ the most for Mode II and the least for Mode I loading. Mixed-Mode I/II fracture toughness is determined in Fixed-Ratio Mixed-Mode and Mixed-Mode Bending tests, performed at the same Mixed-Mode I/II ratio of 4:3. The two test methods yield comparable results for UD GF- and UD CF-epoxy.

OriginalspracheEnglisch
Aufsatznummer111009
Seitenumfang27
FachzeitschriftEngineering Fracture Mechanics
Jahrgang2025
AusgabenummerVolume 320, 13 May
DOIs
PublikationsstatusElektronische Veröffentlichung vor Drucklegung. - 6 März 2025

Bibliographische Notiz

Publisher Copyright:
© 2025 The Author(s)

Schlagwörter

  • Fracture toughness
  • Delamination resistance
  • Glass fiber reinforced polymer laminate
  • Carbon fiber reinforced polymer
  • Mixed-Mode I/II

Dieses zitieren