Zur Hauptnavigation wechseln Zur Suche wechseln Zum Hauptinhalt wechseln

High Area Capacity Lithium-Sulfur Full-cell Battery with Prelitiathed Silicon Nanowire-Carbon Anodes for Long Cycling Stability

  • Andreas Krause
  • , Susanne Dörfler
  • , Markus Piwko
  • , Florian M. Wisser
  • , Tony Jaumann
  • , Eike Ahrens
  • , Lars Giebeler
  • , Holger Althues
  • , Stefan Schädlich
  • , Julia Grothe
  • , Andrea Jeffery
  • , Matthias Grube
  • , Jan Brückner
  • , Jan Martin
  • , Jürgen Eckert
  • , Stefan Kaskel
  • , Thomas Mikolajick
  • , Walter M. Weber
  • Technische Universität Dresden
  • Fraunhofer-Institut für Werkstoff- und Strahltechnik IWS, Dresden
  • IFW Dresden
  • NaMLab gGmbH
  • Erich-Schmid-Institut für Materialwissenschaft der Österreichischen Akademie der Wissenschaften

Publikation: Beitrag in Fachzeitschrift › Artikel › Forschung › Begutachtung

56 Zitate (Scopus)

Abstract

We show full Li/S cells with the use of balanced and high capacity electrodes to address high power electro-mobile applications. The anode is made of an assembly comprising of silicon nanowires as active material densely and conformally grown on a 3D carbon mesh as a light-weight current collector, offering extremely high areal capacity for reversible Li storage of up to 9 mAh/cm2. The dense growth is guaranteed by a versatile Au precursor developed for homogenous Au layer deposition on 3D substrates. In contrast to metallic Li, the presented system exhibits superior characteristics as an anode in Li/S batteries such as safe operation, long cycle life and easy handling. These anodes are combined with high area density S/C composite cathodes into a Li/S full-cell with an ether- and lithium triflate-based electrolyte for high ionic conductivity. The result is a highly cyclable full-cell with an areal capacity of 2.3 mAh/cm2, a cyclability surpassing 450 cycles and capacity retention of 80% after 150 cycles (capacity loss <0.4% per cycle). A detailed physical and electrochemical investigation of the SiNW Li/S full-cell including in-operando synchrotron X-ray diffraction measurements reveals that the lower degradation is due to a lower self-reduction of polysulfides after continuous charging/discharging.
OriginalspracheEnglisch
Aufsatznummer27982
Seitenumfang12
FachzeitschriftScientific reports (London : Nature Publishing Group)
Jahrgang2016
Ausgabenummer6
DOIs
PublikationsstatusVeröffentlicht - 20 Juni 2016

Dieses zitieren