Abstract
The present study deals with the development of a continuous cooling transformation diagram corresponding to the coarse-grained heat-affected zone of a high-strength all-weld metal with a minimum yield strength of 1100 MPa fabricated via gas metal arc welding. Dilatometry tests were conducted to determine the transition temperatures. High-resolution imaging methods, such as transmission electron microscopy and atom probe tomography, as well as nanoindentation, were employed to resolve the microstructural constituents. At fast cooling rates (t 8/5 from 1.4 to 25 s), the microstructure comprises a mixture of martensite and coalesced bainite, with a slight increase in the content of coalesced bainite with faster cooling. This demonstrates that coalesced bainite cannot be avoided in the coarse-grained heat-affected zone of the current alloy by increasing the cooling rate. With slower cooling (t 8/5 ≥ 50 s), the microstructure becomes increasingly bainitic, accompanied by a marginal drop in Vickers hardness. At t 8/5 times of 500 s and 1000 s, the all-weld metal consists of granular bainite with significant amounts of retained austenite and different shaped martensite-austenite constituents. The coarser massive-type constituents contain body-centered cubic grains, sized in the hundreds of nanometers, with a hardness approximately twice as high as that of the surrounding bainitic matrix.
| Originalsprache | Englisch |
|---|---|
| Seiten (von - bis) | 813-823 |
| Seitenumfang | 11 |
| Fachzeitschrift | Welding in the world |
| Jahrgang | 69.2025 |
| Ausgabenummer | March |
| DOIs | |
| Publikationsstatus | Veröffentlicht - 18 Dez. 2024 |
Bibliographische Notiz
Publisher Copyright:© The Author(s) 2024.
UN SDGs
Dieser Output leistet einen Beitrag zu folgendem(n) Ziel(en) für nachhaltige Entwicklung
-
SDG 9 – Industrie, Innovation und Infrastruktur
Dieses zitieren