@article{ce15187fa8924a98bd9717a3b38a3b9a,
title = "Two different correlations between nanoindentation modulus and mineral content in the bone-cartilage interface",
author = "Gupta, \{H. S.\} and S. Schratter and W. Tesch and P. Roschger and A. Berzlanovich and Thomas Sch{\"o}berl and K Klaushofer and P. Fratzl",
year = "2005",
doi = "10.1016/j.jsb.2004.10.010",
language = "English",
volume = "149",
pages = "138--148",
journal = "Journal of structural biology",
issn = "1047-8477",
publisher = "Academic Press Inc.",
}