Cathodic and Anodic Stress Corrosion Cracking of a New High-Strength CrNiMnMoN Austenitic Stainless Steel

  • Mathias Truschner (Speaker)
  • Jacqueline Deutsch (contributor)
  • Andreas Keplinger (contributor)
  • Mori, G. K. (Speaker)

Activity: Talk or presentation Oral presentation

Period10 Jun 2021
Event titleSCI Electrochemistry PGR Conference 2021
Event typeConference
LocationManchester, United KingdomShow on map
Degree of RecognitionInternational