Determining Eutectic Grain Size and Casting Defects in an Al-12Si0.8Cu-0.5Fe-0.9Mg-0.7Ni-0.2Zn Alloy

  • Peter Schumacher (Speaker)
  • LI, J. (contributor)
  • Bernd Oberdorfer (contributor)
  • Daniel Habe (contributor)

Activity: Talk or presentation Oral presentation

Period26 Feb 201717 Mar 2017
Event titleTMS 2017: 146th Annual Meeting & Exhibition
Event typeConference
LocationSan Diego, CA, United StatesShow on map