Spherical Nanoindentation - Prospects towards its application as a multifunctional testing technique
Alexander Leitner (Speaker)
Maier-Kiener, V.
(contributor)
Kiener, D.
(contributor)
Chair of Materials Physics (430)
Chair of Physical Metallurgy (420)
Activity
:
Talk or presentation
›
Oral presentation
Period
4 Oct 2017
Event title
ECI Nanomechanical Testing in Research and Development
Event type
Conference
Location
Dubrovnik, Croatia
Show on map
Degree of Recognition
International
Keywords
spherical nanoindentation
material flow curves