Combination of Nanoindentation and Microscopy for the Examination of Aluminum Alloys in Coarse- and Ultrafine-Grained Condition

Johann Kappacher, Alexander Leitner, Helmut Clemens, Verena Maier-Kiener

Research output: Contribution to journalArticleResearch

Original languageEnglish
Pages (from-to)432-442
Number of pages11
JournalPractical metallography = Praktische Metallographie
Volume56.2019
Issue number7
DOIs
Publication statusPublished - 9 Jan 2019

Cite this