Creep testing of refractories at service related load levels and application for material simulation

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Translated title of the contributionCreep testing of refractories at service related load levels and application for material simulation
Original languageEnglish
Title of host publicationAdvances in Science and Technology
Pages221-225
Publication statusPublished - 2014

Cite this