Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures

  • Xi'an University of Technology

Research output: Contribution to journalArticleResearchpeer-review

11 Citations (Scopus)
Original languageEnglish
Pages (from-to)581-590
Number of pages10
JournalJournal of alloys and compounds
Volume699.2017
Issue number30 March
DOIs
Publication statusPublished - 26 Dec 2016

Cite this