Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten

  • Saurav Goel
  • , Graham Cross
  • , Alexander Stukowski
  • , Ernst Gamsjäger
  • , Ben Beake
  • , Anupam Agrawal
  • School of Aerospace, Transport and Manufacturing, Cranfield Univeristy
  • Crann Nanoscience Institute; Trinity College
  • Technische Universität Darmstadt
  • University of Leeds, School of Earth and Environment
  • Texas A and M University

Research output: Contribution to journalArticleResearchpeer-review

24 Citations (Scopus)
Original languageEnglish
Pages (from-to)196-210
Number of pages15
JournalComputational materials science
Volume152
DOIs
Publication statusPublished - 2018

Keywords

  • MD simulation, Indenter, Nanoindentation, Deformation, Tungsten

Cite this