Effect of weld defects on the fatigue strength of ultra high-strength steels

Markus Ottersböck, Martin Leitner, Michael Stoschka, Wilhelm Maurer

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Original languageEnglish
Title of host publicationProceedings of the ICMFM18
Publication statusPublished - 2016