Examining nanoindentation imprints with in-situ AFM-SEM

  • Megan Cordill
  • , J. Kreith
  • , T. Strunz
  • , E.J. Fantner

Research output: Contribution to conferencePosterResearchpeer-review

Original languageEnglish
Publication statusPublished - 30 Mar 2016
EventSpring Materials Research Society 2016 conference - Boston, United States
Duration: 28 Mar 2016 → …

Conference

ConferenceSpring Materials Research Society 2016 conference
Country/TerritoryUnited States
CityBoston
Period28/03/16 → …