| Translated title of the contribution | FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter |
|---|---|
| Original language | English |
| Title of host publication | 34th International Conference on Metallurgical Coatings and Thin Films |
| Pages | 60-60 |
| Publication status | Published - 2007 |
FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter
- Claudia Walter
- , T. Antretter
- , Rostislav Daniel
- , Christian Mitterer
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution