Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91

Gerhard Gerstmayr, Gregor Mori, Wilfried Eichlseder

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Original languageEnglish
Title of host publicationMagnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition
Pages145-150
Number of pages6
Publication statusPublished - 21 May 2010
EventMagnesium Technology 2010 - TMS 2010 Annual Meeting and Exhibition - Seattle, WA, United States
Duration: 14 Feb 201018 Feb 2010

Publication series

NameMagnesium Technology
ISSN (Print)1545-4150

Conference

ConferenceMagnesium Technology 2010 - TMS 2010 Annual Meeting and Exhibition
Country/TerritoryUnited States
CitySeattle, WA
Period14/02/1018/02/10

Keywords

  • Galvanic corrosion
  • High-strength aluminum bolt
  • Magnesium
  • Stress corrosion cracking