Investigation of Hydrometallurgical Pre-Treatment for the Removal and Decomposition of Electrolyte Residues from Spent NMC/C Lithium-Ion Battery Black Mass

Research output: Thesis › Master's Thesis

Abstract

Lithium-ion batteries are becoming increasingly important as a key enabler of the transition toward a more climate-neutral economy. However, materials, including natural graphite, lithium, and cobalt, which are required for battery-cell production, are classified as critical raw materials by the European Union, reflecting the significant supply risk arising from their predominant sourcing from outside the EU. Recycling of spent lithium-ion batteries represents a key strategy to reduce this dependency by recovering valuable materials from end-of-life cells. For hydrometallurgical recycling, pre-treatment is necessary to reduce impurity loads and therefore improve metal recovery rates. Pyrolysis is commonly employed to remove organic electrolyte and binder residues. However, alternative low-temperature treatments such as vacuum drying are increasingly considered to enable partial electrolyte recovery and reduce toxic off-gas generation, at the cost of higher residual electrolyte loads entering the hydrometallurgical process. This thesis investigates an aqueous pre-washing step applicable to both pyrolyzed and unpyrolyzed black mass, with the aim of combining the selective extraction of lithium with the removal of electrolyte residues prior to hydrometallurgical leaching. The process parameters investigated include extraction times of 120 to 240 min, solid-to-liquid ratios of 50 to 200 g/L, and temperatures of 60 to 80 °C. Additionally, the decomposition of PF6- using aluminum salts is explored, and a sequential combination of both steps is evaluated to assess the feasibility of an integrated pre-treatment process. The pre-washing step demonstrates high selectivity, with no significant dissolution of valuable metals other than lithium. Maximum lithium extraction efficiencies of 44.5 % and 17.2 % are achieved for pyrolyzed and unpyrolyzed black mass respectively, with a maximum organic carbon removal efficiency of 21.2 % recorded for unpyrolyzed black mass. The aluminum-salt treatment applied directly to black mass results in co-extraction of nickel, cobalt, and manganese at levels of approximately 8 %, which are subsequently lost during precipitation. In the sequential combination, lithium dissolved during the pre-washing step is largely retained in solution throughout the aluminum-salt treatment and precipitation, while the dissolved carbon content of the filtrate is simultaneously reduced. These findings demonstrate that sequential pre-washing followed by aluminum-salt treatment of the filtrate is a viable approach, as direct treatment of black mass results in losses of valuable metals.
Translated title of the contributionHydrometallurgische Vorbehandlung zur selektiven Entfernung und Zersetzung von Elektrolytrückständen aus NMC/C Lithium-Ionen-Batterie-Schwarzmasse
Original languageEnglish
QualificationDipl.-Ing.
Awarding Institution
  • Montanuniversität
Supervisors/Advisors
  • Gerold, Eva, Supervisor (internal)
  • Lerchbammer, Reinhard, Co-Supervisor (internal)
Award date26 Jun 2026
DOIs
Publication statusPublished - 2026

Bibliographical note

embargoed until 08-05-2031

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 7 - Affordable and Clean Energy
    SDG 7 Affordable and Clean Energy
  2. SDG 13 - Climate Action
    SDG 13 Climate Action

Keywords

  • Hydrometallurgy
  • Lithium-ion battery recycling
  • Electrolyte residues
  • Hexafluorophosphate
  • Ethylene carbonate
  • Pre-washing
  • Aluminum-salt treatment

Cite this