Metadynamic recrystallization of the nickel-based superalloy Allvac 718Plus™

  • Technische Universität Graz
  • Böhler Schmiedetechnik GmbH and Co KG
  • Christian Doppler Labor für Werkstoffmodellierung und Simulation

Research output: Chapter in Book/Report/Conference proceeding › Conference contribution

4 Citations (Scopus)
Original languageEnglish
Title of host publicationTHERMEC 2009
EditorsTara Chandra, Tara Chandra, Tara Chandra, N. Wanderka, N. Wanderka, N. Wanderka, Walter Reimers, Walter Reimers, Walter Reimers, M. Ionescu, M. Ionescu, M. Ionescu
PublisherTrans Tech Publications
Pages2327-2332
Number of pages6
ISBN (Print)0878492941, 9780878492947
DOIs
Publication statusPublished - 2010
Event6th International Conference on Processing and Manufacturing of Advanced Materials - THERMEC'2009 - Berlin, Germany
Duration: 25 Aug 2009 → 29 Aug 2009

Publication series

NameMaterials Science Forum
Volume638-642
ISSN (Print)0255-5476
ISSN (Electronic)1662-9752

Conference

Conference6th International Conference on Processing and Manufacturing of Advanced Materials - THERMEC'2009
Country/TerritoryGermany
CityBerlin
Period25/08/09 → 29/08/09

Keywords

  • FEM
  • Metadynamic recrystallization
  • Superalloy

Cite this