Microchemistry Evolution in 8xxx Aluminium Foil Stock Alloys during Thermo-mechanical Processing

  • Erik Santora

Research output: Thesis › Doctoral Thesis

Abstract

The objective of this work was to investigate the effects of the thermo-mechanical processing steps in the production of 8xxx foil stock alloys, on the evolution of the microstructure and microchemistry, i.e. phase transformations, dispersoid precipitation and the content of elements in solid solution, on a laboratory-scale, supported by CALPHAD simulations.
First, as-cast samples from an EN AW-8079 ingot were characterized, showing a strong cooling rate dependence of the microstructure and microchemistry, resulting in differences in the type and distribution of the predominant intermetallic phases, and thus in different mechanical properties after rolling. It has also been shown that higher Fe alloy contents could increase the strength of the material and Ti additions improve the effectiveness of the applied grain refiner rods.
Homogenization annealing treatments resulted in precipitations that reduced the solute content below 500 °C, followed by increases due to dispersoid dissolution and phase transformations at increasing temperatures up to a maximum at 550 °C and 595 °C in EN AW-8011 and EN AW-8079, respectively, before decreasing at higher temperatures or subsequent holding and/or cooling periods. Overall, continuous dispersoid particle growth and coarsening of the constituent particles was observed.
The effects of hot deformation on dynamic precipitation in EN AW-8079 specimens were inconclusive, due to statistical limitations of the methods used, but some indications were found. However, homogenization treatments were found to have a strong effect on the hot workability, due to solid solution strengthening, and high-temperature homogenization effectively retard the static recovery or recrystallization after hot deformation.
Intermediate annealing of cold-rolled EN AW-8079 sheet showed complete softening at temperatures above 300 °C, while the ongoing recrystallization is associated with the depletion of the elements in solute solution. High annealing temperatures maximized the content of elements in solid solution, exceeding the initial level before inter-annealing, while subsequent cooling led to a decrease in the content of elements in solid solution, both being attributed to dissolution or precipitation of Si or α-AlFeSi dispersoid particles, respectively.
Finally, the potential of process design schemes for targeted softening behavior or thermostability of the foil stock sheet and thus the final foil product were identified, and potential follow-up questions were defined.
Translated title of the contributionEntwicklung der Mikrochemie von 8xxx Aluminium-Vorwalzband entlang der thermomechanischen Prozesskette
Original languageEnglish
QualificationDr.mont.
Awarding Institution
  • Montanuniversität
Supervisors/Advisors
  • Uggowitzer, Peter, Assessor A (internal)
  • Hirsch, Jürgen, Assessor B (external), External person
  • Antrekowitsch, Helmut, Co-Supervisor (internal)
  • Pogatscher, Stefan, Supervisor (internal)
DOIs
Publication statusPublished - 2025

Bibliographical note

embargoed until 21-01-2030

Keywords

  • 8xxx Aluminium foil stock
  • Casting
  • Homogenisation
  • Hot forming
  • Intermediate annealing
  • Microstructure&Microchemistry
  • Thermal stability