TY - JOUR
T1 - Microstructure, mechanical and thermo-physical properties of CVD TiCxN1-x coatings on cemented carbide substrates grown with C2H6 as C feeding precursor
AU - Kainz, Christina
AU - Schalk, Nina
AU - Tkadletz, Michael
AU - Winkler, Markus
AU - Czettl, Christoph
N1 - Publisher Copyright:
© 2020 Elsevier B.V.
PY - 2020/7/25
Y1 - 2020/7/25
N2 - The established industrial processes used for the growth of TiC
xN
1-x coatings by chemical vapor deposition (CVD) suffer from substantial limitations, either in regard of brittle phase formation or restriction in the C/(C + N) ratio. Using the alternative C precursor C
2H
6 allows to overcome these issues. Thus, within this work, the microstructure, phase composition, micro-mechanical and thermo-physical properties of CVD TiC
xN
1-x coatings grown with C
2H
6 were investigated. Through adjustment of the C
2H
6 and N
2 flow in the feed gas, the C/(C + N) ratio in the coatings was varied between pure TiN and TiC
0.80N
0.20. All coatings are characterized by a single-phase face centered cubic structure. The 〈110〉 fiber texture present in all coatings becomes more pronounced with increasing C content. None of the investigated coatings showed thermal cracks on the surface. The thermal conductivity decreases with addition of C from 45 ± 5 W/mK in TiN to 32 ± 3 W/mK in all ternary TiC
xN
1-x coatings. TiC
0.47N
0.53 exhibits the highest hardness (30.0 ± 1.4 GPa), while TiC
0.63N
0.36 turned out as the stiffest coating with a Young's modulus of 576 ± 23 GPa. The fracture stress σ
F and toughness K
IC are superior in coatings with moderate C and N content, with TiC
0.63N
0.37 being the strongest (σ
F = 7.7 ± 0.4 GPa) and TiC
0.47N
0.53 (K
IC = 4.4 ± 0.3 MPa m
1/2) the toughest within this series. Coatings with moderate to high C content were found to exhibit a microstructure provoking a lower thermal conductivity and improved mechanical properties compared to those with a low C/(C + N) ratio.
AB - The established industrial processes used for the growth of TiC
xN
1-x coatings by chemical vapor deposition (CVD) suffer from substantial limitations, either in regard of brittle phase formation or restriction in the C/(C + N) ratio. Using the alternative C precursor C
2H
6 allows to overcome these issues. Thus, within this work, the microstructure, phase composition, micro-mechanical and thermo-physical properties of CVD TiC
xN
1-x coatings grown with C
2H
6 were investigated. Through adjustment of the C
2H
6 and N
2 flow in the feed gas, the C/(C + N) ratio in the coatings was varied between pure TiN and TiC
0.80N
0.20. All coatings are characterized by a single-phase face centered cubic structure. The 〈110〉 fiber texture present in all coatings becomes more pronounced with increasing C content. None of the investigated coatings showed thermal cracks on the surface. The thermal conductivity decreases with addition of C from 45 ± 5 W/mK in TiN to 32 ± 3 W/mK in all ternary TiC
xN
1-x coatings. TiC
0.47N
0.53 exhibits the highest hardness (30.0 ± 1.4 GPa), while TiC
0.63N
0.36 turned out as the stiffest coating with a Young's modulus of 576 ± 23 GPa. The fracture stress σ
F and toughness K
IC are superior in coatings with moderate C and N content, with TiC
0.63N
0.37 being the strongest (σ
F = 7.7 ± 0.4 GPa) and TiC
0.47N
0.53 (K
IC = 4.4 ± 0.3 MPa m
1/2) the toughest within this series. Coatings with moderate to high C content were found to exhibit a microstructure provoking a lower thermal conductivity and improved mechanical properties compared to those with a low C/(C + N) ratio.
UR - http://www.scopus.com/inward/record.url?scp=85085268457&partnerID=8YFLogxK
U2 - 10.1016/j.surfcoat.2020.125868
DO - 10.1016/j.surfcoat.2020.125868
M3 - Article
SN - 0257-8972
VL - 394.2020
JO - Surface & coatings technology
JF - Surface & coatings technology
IS - 25 July
M1 - 125868
ER -