| Translated title of the contribution | Mikrostruktur einer C/C-Cu Verbindung für Erste Wand Komponenten des Iter |
|---|---|
| Original language | German |
| Title of host publication | Fortschritte in der Metallographie 38 |
| Publisher | Werkstoff-Informationsges. |
| Pages | 525-530 |
| Publication status | Published - 2006 |