Nanoindentation creep behavior of an Fe–Cr–Mo–B–C amorphous coating via atmospheric plasma spraying

  • Quan Dong
  • , Jun Tan
  • , Rui Huang
  • , Hailian Wang
  • , Peng Song
  • , C. J. Li
  • , Z. X. Feng
  • , Mariana Calin
  • , Jürgen Eckert
  • College of Materials Science and Engineering
  • Kunming University of Science and Technology
  • Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province)
  • Leibniz Institute for Solid State and Materials Research, Dresden
  • Erich Schmid Institute of Materials Science

Research output: Contribution to journal › Article › Research › peer-review

3 Citations (Scopus)
Original languageEnglish
Article number107411
Number of pages9
JournalIntermetallics
Volume141.2022
Issue numberFebruary
Early online date11 Nov 2021
DOIs
Publication statusPublished - Feb 2022

Bibliographical note

Publisher Copyright: © 2021 Elsevier Ltd

Keywords

  • Amorphous coating
  • Nanoindentation creep
  • Shear transformation zone
  • Strain rate sensitivity