Nanoindentation of chemical-vapor deposited Al2O3 hard coatings at elevated temperatures

  • Marisa Rebelo De Figueiredo
  • , Manuel D. Abad
  • , Adrian J. Harris
  • , Christoph Czettl
  • , Christian Mitterer
  • , Peter Hosemann

Research output: Contribution to journalArticleResearchpeer-review

26 Citations (Scopus)
Original languageEnglish
Pages (from-to)20-24
JournalThin solid films
Volume578
DOIs
Publication statusPublished - 2015