Nanoindentation of wet and dry compact bone: Influence of environment and indenter tip geometry on the indentation modulus

Ingomar Jäger, G. Guidoni, M. Swain

Research output: Contribution to journalArticleResearchpeer-review

30 Citations (Scopus)
Translated title of the contributionNanoindentation of wet and dry compact bone: Influence of environment and indenter tip geometry on the indentation modulus
Original languageEnglish
Pages (from-to)553-565
JournalPhilosophical magazine
Publication statusPublished - 2010