Resistance to stress corrosion cracking of a new high strength stainless steel wire material

  • Mathias Truschner
  • , Anton Trautmann (Co-editor)
  • , Jacqueline Deutsch (Co-editor)
  • , Gregor Karl Mori (Co-editor)
  • , Andreas Keplinger (Co-editor)

Research output: Contribution to conferencePosterResearch

Original languageEnglish
Publication statusPublished - 7 Sept 2020
EventEurocorr 2020: Virtual Eurocorr - Online
Duration: 7 Sept 202011 Sept 2020