Skip to main navigation Skip to search Skip to main content

TENSILE AND COMPRESSIVE CREEP TESTING OF REFRACTORIES AT SERVICE RELATED LOADS

Research output: Chapter in Book/Report/Conference proceedingConference contribution

1 Citation (Scopus)
Original languageEnglish
Title of host publicationUNITERC 2015
Editors 14th Biennial Worldwide Congress
Number of pages1
ISBN (Electronic)978-3-9815813-1-7
Publication statusPublished - 2015

Keywords

  • Thermal shock resistance

Cite this