The Effect of Surface Roughness on Nanoindentation of Hard Coatings: Simulation and Experiment

Claudia Walter, Christian Mitterer

Research output: Contribution to conferencePosterResearchpeer-review

Translated title of the contributionThe Effect of Surface Roughness on Nanoindentation of Hard Coatings: Simulation and Experiment
Original languageEnglish
Publication statusPublished - 2009
EventNanomechanical Testing in Materials Research and Development - Barga, Italy
Duration: 11 Oct 200916 Oct 2009