Skip to main navigation Skip to search Skip to main content

The microstructure of heat-treated nickel-based superalloy 718Plus

  • Lawrence Whitmore
  • , Mohammed Reza Ahmadi
  • , Laure Guetaz
  • , Harald Leitner
  • , Erwin Povoden-Karadeniz
  • , Martin Stockinger
  • , Ernst Kozeschnik

Research output: Contribution to journalArticleResearchpeer-review

21 Citations (Scopus)
Translated title of the contributionThe microstructure of heat-treated nickel-based superalloy 718Plus
Original languageEnglish
Pages (from-to)39-45
JournalMaterials science and engineering: A, Structural materials: properties, microstructure and processing
Volume610
DOIs
Publication statusPublished - 2014