Skip to main navigation Skip to search Skip to main content

Undercooling of Superalloy Melts: Basis of a New Manufacturing Technique for Single-Crystal Turbine Blades

Research output: Contribution to journalArticleResearchpeer-review

28 Citations (Scopus)
Translated title of the contributionUndercooling of Superalloy Melts: Basis of a New Manufacturing Technique for Single-Crystal Turbine Blades
Original languageEnglish
Pages (from-to)299-303
JournalMaterials science and engineering: A, Structural materials: properties, microstructure and processing
Publication statusPublished - 1994