Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting. / Attar, Hooyar; Ehtemam-Haghighi, S.; Kent, D.; Okulov, I. V.; Wendrock, H.; Bönisch, Matthias; Volegov, A. S.; Calin, Mariana; Eckert, Jürgen; Dargusch, M.S.

in: Materials science and engineering: A, Structural materials: properties, microstructure and processing, Jahrgang 688, 03.2017, S. 20-26.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Harvard

APA

Attar, H., Ehtemam-Haghighi, S., Kent, D., Okulov, I. V., Wendrock, H., Bönisch, M., Volegov, A. S., Calin, M., Eckert, J., & Dargusch, M. S. (2017). Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting. Materials science and engineering: A, Structural materials: properties, microstructure and processing, 688, 20-26.

Author

Attar, Hooyar ; Ehtemam-Haghighi, S. ; Kent, D. ; Okulov, I. V. ; Wendrock, H. ; Bönisch, Matthias ; Volegov, A. S. ; Calin, Mariana ; Eckert, Jürgen ; Dargusch, M.S. / Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting. in: Materials science and engineering: A, Structural materials: properties, microstructure and processing. 2017 ; Jahrgang 688. S. 20-26.

Bibtex - Download

@article{3802b94621874620bef357ea4d261750,
title = "Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting",
author = "Hooyar Attar and S. Ehtemam-Haghighi and D. Kent and Okulov, {I. V.} and H. Wendrock and Matthias B{\"o}nisch and Volegov, {A. S.} and Mariana Calin and J{\"u}rgen Eckert and M.S. Dargusch",
year = "2017",
month = mar,
language = "English",
volume = "688",
pages = "20--26",
journal = "Materials science and engineering: A, Structural materials: properties, microstructure and processing",
issn = "0921-5093",
publisher = "Elsevier BV",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting

AU - Attar, Hooyar

AU - Ehtemam-Haghighi, S.

AU - Kent, D.

AU - Okulov, I. V.

AU - Wendrock, H.

AU - Bönisch, Matthias

AU - Volegov, A. S.

AU - Calin, Mariana

AU - Eckert, Jürgen

AU - Dargusch, M.S.

PY - 2017/3

Y1 - 2017/3

M3 - Article

VL - 688

SP - 20

EP - 26

JO - Materials science and engineering: A, Structural materials: properties, microstructure and processing

JF - Materials science and engineering: A, Structural materials: properties, microstructure and processing

SN - 0921-5093

ER -