Essential refinements of spherical nanoindentation protocols for the reliable determination of mechanical flow curves

Research output: Contribution to journalArticleResearchpeer-review

Details

Original languageEnglish
Pages (from-to)69-80
Number of pages12
JournalMaterials and Design
Volume146
DOIs
StatePublished - 15 May 2018