Exploring the mechanical character of molybdenum grain boundaries via nanoindentation and three-point-bending

Research output: Contribution to conferencePosterResearch

External Organisational units

  • PLANSEE SE
  • Erich Schmid Institute of Materials Science

Details

Original languageEnglish
Publication statusPublished - 2019
EventECI Nanomechanical Testing in Materials Research and Development - Torremolinos, Spain
Duration: 29 Sep 20194 Oct 2019

Conference

ConferenceECI Nanomechanical Testing in Materials Research and Development
CountrySpain
CityTorremolinos
Period29/09/194/10/19