Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation

Research output: Contribution to journalArticleResearchpeer-review

Standard

Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation. / Merle, Benoit; Maier-Kiener, Verena; Pharr, George M.

In: Acta materialia, Vol. 134, 2017, p. 167-176.

Research output: Contribution to journalArticleResearchpeer-review

Bibtex - Download

@article{63ec50e97dae4baf8b4fbd2926f9d198,
title = "Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation",
author = "Benoit Merle and Verena Maier-Kiener and Pharr, {George M.}",
year = "2017",
doi = "http://dx.doi.org/10.1016/j.actamat.2017.05.036",
language = "English",
volume = "134",
pages = "167--176",
journal = "Acta materialia",
issn = "1359-6454",
publisher = "Elsevier BV",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation

AU - Merle, Benoit

AU - Maier-Kiener, Verena

AU - Pharr, George M.

PY - 2017

Y1 - 2017

U2 - http://dx.doi.org/10.1016/j.actamat.2017.05.036

DO - http://dx.doi.org/10.1016/j.actamat.2017.05.036

M3 - Article

VL - 134

SP - 167

EP - 176

JO - Acta materialia

JF - Acta materialia

SN - 1359-6454

ER -